Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin GTX910 - Europe - (PPE+PA*) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin GTX910 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl GTX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
NORYL GTX™ 910 resin is non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). NORYL GTX910 resin exhibits excellent chemical resistance and is an excellent candidate for automotive applications such as plastic/metal hybrid components, rail extensions, crash cans, wheel covers, and energy absorbers.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 10 cm³/10min ISO 1133
온도 280 °C -
하중 5 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2200 MPa ISO 527
항복강도 55 MPa ISO 527
항복변형률 8 % ISO 527
파단시 강도 50 MPa ISO 527
파단시 신율 25 % ISO 527
굴곡 계수 1900 MPa ISO 178
챠피 노치드 충격 강도, +23°C 25 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 12 kJ/m² ISO 179/1eA
아이조드 노치 충격 강도, +23°C, 4mm 25 kJ/m² ISO 180/1A
아이조드 노치 충격 강도, -30°C, 4mm 12 kJ/m² ISO 180/1A
Ball indentation hardness 115 MPa ISO 2039-1
열적 특성단위시험규격
ISO 데이터
비카트 연화 온도, A 238 °C ISO 306
비카트 연화 온도, B 195 °C ISO 306
비카트 연화 온도, 120°C/h 50N 195 °C ISO 306
선형 열팽창 계수, 평행 90 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 90 E-6/K ISO 11359-1/-2
열전도율 0.23 W/(m K) DIN 52616
기타 특성단위시험규격
물에서의 흡수성 3.5 % ISO 62와 유사
조건에서의 흡습성 1 % ISO 62와 유사
밀도 1100 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 100 - 120 °C -
Pre-drying - Time 2 - 3 h -
Processing humidity ≤0.07 % -
용융수지온도 280 - 310 °C -
성형온도 80 - 120 °C -
Feed temperature 60 - 80 °C -
Zone 1 260 - 280 °C -
Zone 2 270 - 290 °C -
Zone 3 280 - 300 °C -
특징
생산 공정
사출 성형
응용
자동차의
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.